Ultra-Fine Particle Size: PVC paste resin features extremely small primary particles (0.2–2 μm) and finished particle sizes of 30–80 μm, ensuring uniformity and excellent processing performance.
Excellent Dispersibility in Plasticizers: The resin can easily break down into primary particles when mixed with plasticizers, forming a smooth and stable paste, which is ideal for coating and molding applications.
Stable Paste Formation: When dispersed, it creates a consistent, paste-like fluid with good stability, supporting precise processing and high-quality end products.
High Processing Versatility: Its fine powder form and paste-forming ability make it suitable for a wide range of applications requiring controlled viscosity and smooth surface finishes.
製品説明
Products Description of Polyvinyl Chloride Paste Resin CAS#9002-86-2
Polyvinyl chloride (PVC) is a widely used thermoplastic polymer made from vinyl chloride monomers. Key properties: white-light yellow powder, density 1.35–1.40, chlorine content 56–58%, mp 70–85 °C, excellent chemical resistance, poor thermal/light stability. Available in plasticized soft and unplasticized rigid grades. Used in pipes, wire insulation, films, construction materials and consumer goods.
Product Application of Polyvinyl Chloride Paste Resin CAS#9002-86-2
PVC is a cost-effective, versatile plastic requiring performance-specific additives. Rigid grades are used in chemical equipment, construction and agriculture; flexible grades in wires, cables, films and consumer goods. Additional applications include foam insulation, artificial leather, thermoplastic elastomer seals and chlorofibers (with reported therapeutic benefits for arthritis).